Step 2: Crack Repair
Before applying an Ultra Surface Polymer Concrete texture coat or 1/4" Stamping application, all structural moving cracks should be repaired with the Ultra Surface Crack Repair System as shown below.
(Note: For the 1/4" Stamping System only, the expansion joints will also need to be repaired with this crack repair system, and then cut back open the day after stamping.)
|
|
Fig. 1
Clean cracks during surface preparation.
|
|
|
|
Fig. 2
Clean cracks during surface preparation.
|
|
|
|
Fig. 3
Scrape excess Epoxy off the surface. |
|
|
|
Fig. 4
Apply Elastomeric Basecoat over crack repairs. |
|
|
|
Fig. 5
Immediately apply 4" Crack Repair Fabric over the Elastomeric Basecoat while still wet. |
|
|
|
Fig. 6
Immediately apply another coat of Elastomeric Basecoat over the 4" Crack Repair Fabric. |
|
|
Fig. 7
Apply a patch coat of Ultra Surface Polymer Concrete over the crack repairs. This step is not necessary when doing 1/4" Stamping. |
|